Always thoroughly clean oxidation off. Degrease then clean with SS wire brush , steel wool, or Scotch Bright pad. Preheat, flux,solder. Since you said you're using plumbers solder 50/50? 60/40? The new Antimony Tin Silver stuff is a bit tricky to get a good flow. Flux: use No Corrode solder paste (the brownish stuff) No brainer.
|